        Toady, I ran the 24 hour deposition through the IR and saw that the peaks were in the correct spots.  Since the monolayers formed, I rinsed the cobalt coupons in THF for 15 minutes.  I also made another solution to use on the cobalt coupons.  My solution was octadecylcarboxylic acid using THF as the solvent.   My solution was okay so I started a 24 hour deposition in ODCA.
        Tomorrow, I plan on checking the 24 hour ODPA and ODCA depositions. 